Description

Self-polishing antifouling containing a combination of copper compounds and biocides. After about a week in the final colour-changing immersion. For its self-cleaning properties the product retains its effectiveness throughout the service period.

DESCRIPTION:
HEMPEL's MILLE NCT is a self-polishing antifouling containing a combination of copper compounds and biocides. For its self-cleaning properties the product retains its effectiveness throughout the service period. However the color of the antifouling, one week after soaking in water, can take on a green copper gradient.

RECOMMENDED USE:
Antifouling paint for boats in fiberglass, wood, plywood and ferro-cement. Not suitable for aluminium and light alloys. Risk of corrosion in case of direct contact. Suitable for temperate or cold water.

PHYSICAL CONSTANTS:
Finish: Semi-matt Top Coat
Solids by volume,%: 54 ± 1
Theoretical yield: 13.5 m²/litre to 40 microns
Flash point: 35° C
Specific weight: 1.4 kg/litre
Touch dry: 4 hours at 20° C-8 hours at 10° C
V.O.C.: 405 g/litre

Physical constants are derived from formulas approved by HEMPEL. They are subject to normal manufacturing tolerances and, where indicated, to standard deviations according to ISO 3534-1.

APPLICATION NOTES:

Application method: spray airless spray air Brush/roller/Pad (see notes overleaf)
Diluent (max. vol.): 0808 (5) 0808 (15) 0808 (5)
Nozzle diameter:. 018 "-. 023"
Nozzle pressure: 150 bar/2175 psi (data for the Airless spray are indicative and subject to adjustments)
Tools cleaning: HEMPEL's THINNER 0808
Recommended thickness: 40 microns dry
Recommended thickness, wet: 75 microns
Covering range, min: 5 hours at 20° C-9 hours at 10° C
Covering, max interval: none (see notes overleaf)

SURFACE PREPARATION:

Previous: antifouling

Remove oil, grease, etc with HEMPEL's YACHT CLEANER
67601, followed by high pressure washing with fresh water, even to remove.
Antifouling exhausted during posting. The surface must be completely dry before coating. The application of one coat of sealant depends on the type and condition of existing antifouling.

CONDITIONS OF APPLICATION:
The surface must be completely dry and clean. Apply only in dry weather. The surface temperature must be above the dew point to prevent condensation.
The temperature of the paint should be above 15° c. Avoid the application in direct sunlight. In enclosed spaces provide adequate ventilation during application and drying.

PREVIOUS HAND:
HEMPEL's YACHT 26030 PRIMER or HEMPEL's LIGHT 45551 PRIMER or as per specification.
NEXT HAND: No

NOTES:
The antifouling paint containing pigments with high specific gravity and must be mixed thoroughly prior to use. Dilute at least for proper formation of paint film thickness recommended.

Recommended number of rounds:
Airless spray application: 2-3 coats with a total thickness of 120 microns
Air spraying, brush, roller or pad: 3-5 hands
For vessels in excess of 15 knots, apply an additional coat.
The launch should take place after at least 24 hours after application of the last coat. HEMPEL's MANY NTC can stay ashore until 3 months after the painting. If you apply an additional coat of HEMPEL's MANY NTC, after prolonged exposure to atmospheric agents, carefully clean the surface with high-pressure wash and leave