Hempel Hard Racing TecCel Antfouling 2.5Lt 10000 White is a hard matrix antifouling containing high performance TecCel forming a smooth low friction. For boats with a wide speed range.
Price:
€99.91
Listing:
€158.60
You Save:
€58.69 (37%)

Description

Hempel Hard Racing TecCel Antfouling 2.5 Lt 10000 White

HARD RACING TecCel is an antifouling for boats with a wide speed range.
Particularly suitable for powerboats. Do not use on aluminium hulls or light alloy.
Risk of corrosion in case of direct contact. For cold water, warm and hot.

PHYSICAL CONSTANTS:
Tint/Color: 10000 White;
Matt Finish;
Volume solids,% 49 ± 1;
Spreading rate: 12.3 m2/l [sq.ft./US gallon 493.2]-40 micron/1.6 mils;
VOC content g/l 440 [3.6 lb/galloni USA];
Dry to the touch about 4 hour (s) 20° C/68° F;
Approx 8. hour (s) 10° C/50° F;
Specific gravity 1.6 kg/litro [13.2 lb/galloni USA];
Flash point° C 28 [82.4° F];
Pack: 2.5 lt.

APPLICATION DETAILS:
Airless spray application method/Pennello/Rullo/Tampone/spray paint
Diluent, (max volume) 08081 (5%)/(5%)/08081 08081 (5%)
Nozzle hole-0.023 0.018 "
Nozzle pressure 150 bar [2175 psi] (data for airless spray are indicatrivi and subject to adjustments)
Cleaning equipment HEMPEL's THINNER 08081
Dry thickness indicated 40 micron [1.6 mils]
Wet thickness indicated 75 micron [3 mils]
Overcoating interval, min as specified
Overcoating interval, max as specified

SURFACE PREPARATION:
Existing self-polishing antifouling or ablative:
remove any oil or grease, etc. with appropriate detergent(HEMPEL's PRE-CLEAN 67602) and clean with fresh water at high pressure to ensure the complete removal ofany casting antifouling. Let dry before covering.
Hard matrix antifouling exists: Sand to remove the old layer.
Remove any oil or grease, etc. with appropriate detergent (HEMPEL's PRE-CLEAN 67602) and clean with fresh water at high pressure to ensure the complete removal of any casting antifouling. Let dry before covering.
Use sealant or less a coat of sigillante/tie coat depends on the type and condition of existing antifouling.